The medium fusing porcelain system had been developed over several years in cooperation with Makoto Yamamoto and features a natural scattering and reflection of light (halo effect).
Compatible with Lamina Vest and other refractory materials in C.T.E range of 13.8 - 14.4 to produce all ceramic veneers, inlays and onlays.
Feldspar porcelain components (C.T.E. 13.0).
Matches any metal in the C.T.E range of: 13.8 - 15.0 .
The best range for Halo is a metal with a C.T.E with 13.8 - 14.6. Slow cool necessary above 14.6 - 15.0. Compatible with alloys which have a silver contend < 40%.
High temperature for Dentin / Body bake 910 - 930C .